Kennametal KC7512 | Wolframkarbid | Binder Composition | Trägermetall% | Density g/cm³ | Härte, HV | Korngröße |
MN0 | 94.0 | Kobalt | 6.0 | 14,90 | 1350 | Grob |
MN04 | 90.5 | 9,5 | 14,50 USD | 1230 | Grob | |
MN05 | 86.5 | 13,5 | 14.15 | 1100 | Grob | |
MN1 | 86.5 | 13,5 | 14.15 | 970 | Extra Coarse | |
MN2 | 85.0 | 15.0 | 14.05 | 950 | Extra Coarse | |
MN3 | 83.0 | 17.0 | 13.85 | 890 | Extra Coarse | |
MN4 | 80.0 | 20,0 | 13.55 | 830 | Extra Coarse | |
MN5 | 75.0 | 25.0 | 13.10 | 730 | Extra Coarse | |
MN6 | 70.0 | 30.0 | 12.75 | 670 | Extra Coarse | |
BN45 | 88.0 | Co-Ni-Cr | 12.0 | 14.25 | 1075 | Grob |
RCV3 | 85.0 | 15.0 | -14.00 | 1090 | Grob | |
BN55 | 85.0 | 15.0 | -14.00 | 950 | Grob | |
RCV4 | 80.0 | 20,0 | 13.50 | 930 | Grob | |
BN65 | 80.0 | 20,0 | 13,5 | 870 | Grob | |
RCV5 | 75.0 | 25.0 | 13.05 | 800 | Grob | |
RCV6 | 70.0 | 30.0 | 12.70 | 670 | Grob |